Bolt property classes 8.8, 10.9 and 12.9: what they mean and how to choose

Three hex bolts marked with property classes 8.8, 10.9 and 12.9 — illustration

Markings such as 8.8, 10.9 and 12.9 identify a bolt's mechanical property class. They help describe strength requirements, but a complete order also needs dimensions, the product standard, material, coating and assembly requirements.

What do the two numbers mean?

For carbon and alloy steel bolts covered by ISO 898-1, the first number multiplied by 100 indicates nominal tensile strength in MPa. The second number divided by 10 gives the nominal ratio of yield strength to tensile strength. Class 8.8 therefore corresponds to nominal values of 800 MPa and 640 MPa.

Nominal values used in the class designation
ClassTensile strengthYield strength
8.8800 MPa640 MPa
10.91000 MPa900 MPa
12.91200 MPa1080 MPa

These figures explain the designation. They are not allowable loads for an assembled joint. Minimum standard values may differ and may depend on diameter. Do not turn these values into a load rating for a complete connection. Refer to Bossard's technical information on ISO 898-1 for the relevant requirements.

Start with the machine specification

For maintenance work, consult the parts list or approved joint specification. A specified class is part of the technical requirement. A replacement that looks like the removed bolt has not necessarily been verified.

For a new design, agree the choice with the person responsible for the assembly. Purchasing can collect the specification, compare available products and confirm delivery. Availability alone should not determine the property class.

Can a higher class replace the specified class?

Do not treat a higher marking as automatic approval. Check the complete joint, including the mating nut or tapped component, bearing surface, washer and assembly procedure. Have the proposed alternative approved and record that approval for future orders.

For example, if an M10 × 40 bolt in class 8.8 is specified and a supplier offers class 10.9, send the complete alternative specification and current tightening procedure to the responsible engineer. This supports an assessment of the actual change.

Property class alone does not determine tightening torque

Friction, surface condition and assembly method also affect the relationship between torque and clamp force. Coating and lubrication matter. Use the approved machine procedure rather than copying a number from a table based on different conditions. Bossard's guide to tightening methods explains friction scatter and assembly uncertainty.

What should your enquiry include?

  • Product standard, head and drive type.
  • Diameter, thread pitch, length and required threaded length.
  • Property class, material and coating.
  • Application, documentation requirements and approved alternatives.
  • Quantity, deadline and expected repeat demand.

Mark unknown parameters as unknown. A clear head-marking photograph and a drawing extract help identify the product. State whether it is needed for emergency maintenance, a prototype or regular production.

Frequently asked questions

Does colour identify the property class?

No. Treat coating and strength requirements as separate entries and confirm them with product documentation.

Does M8 mean class 8.8?

No. M8 identifies a metric thread size; 8.8 identifies mechanical properties.

What if the old marking is unreadable?

Consult the machine documentation. Photographs and measurements assist identification but cannot establish a worn part's mechanical properties.

Send Śrub-Top your specification to check product availability. Joint requirements should come from the approved technical documentation.

The generated illustration is not a photograph of a specific batch or a technical product drawing.